Hello all.
Wondering if anyone out there has experience with SW ext oil gloss applications below 50 degrees. yes in the ideal world it woujldnt be reccomended but this is how the cards fell.
HO had whole exterior painted in 06. now in 09 most of it is peeling and flaking. i got out there late in the season, managed to strip down to bare wood the worst areas, remove and re caulk, double coat with BM penetrating aklyd primer and now the SW ext oil which is what inherited and due to sheen variations off other products i dont want to switch at this stage in the game.
Trim color went on yesterday temps hovering right bout 50, over night and today dipped to low to mid 40`s. finnish still tacky, areas where done last wet. contemplated putting on the rest today but have reservations as i havent used this product before.. obviously the best would be to wait until nicer weather..but im in the midwest where u sneeze and it changes.
any one had to put it on below 50 deg and if so how did it effect the product in the short run and long run that was noticed.
thanks
|